178 Outstanding Abrasion Resitance At High Temparature At 1400F Complex Carbides Polarity Dcep Harness 63-66Rc Number Of Passes 2
(Pack of
5)
Ultra-Brade SD utilizes a complex carbide alloy system that provides outstanding abrasion resistance even at high temperatures.
Tubular electrode design provides 90% deposition efficiency
Reduces smoke by half compared to conventional hardfacing electrodes
Runs at lower amperage reduces distortion, weld dilution andmetal fatigue
Hardness of up to 66 Rc, one layer can outlast two layers of competitive product
Designed to withstand extreme temperature abrasion up to 1400˚F (760˚C)
Not designed for impact resistance
Hardness: 63-66 Rc (deposits will relief check crack readily) Max deposit thickness: 2 layersCurrent: DCEP (DC+) or AC Abrasion resistance: Excellent ASTM G65 Procedure A (Dry sand rubber wheel abrasion test):- 10.51 mm3 volume loss- 0.072 gm mass loss For comparison sintered tungsten carbide: 0.039 to 0.080 gm mass loss
Frequently Bought Together
7355 Carbide Hard Facing Stick Rod Electrode 1/4"
Couldn't load pickup availability
706 Hard Facing Buildup MIG Welding Wire 0.045"
Couldn't load pickup availability
7770 Hard Facing Buildup Stick Rod Electrode 1/8"
Couldn't load pickup availability
174 Gray High Abrasion Moderate Impact 1/8
Couldn't load pickup availability
7220 Carbide Hard Facing Stick Rod Electrode 3/8"
Couldn't load pickup availability
711 Carbide Hard Facing Stick Rod Electrode 5/32"
Couldn't load pickup availability
Drive Rivet Nylon M8
Couldn't load pickup availability
Inner Fender Shield Attaching Clip Nylon Black
Couldn't load pickup availability
Cowl Bumper Fender Liner/Engine Under Cover Rivet
Couldn't load pickup availability
Cronatron Welding Guide
Couldn't load pickup availability
Heat Stick 400F Degrees
Couldn't load pickup availability
710 Stainless Steel Electrode 3/32"
Couldn't load pickup availability
Product Description
Ultra-Brade SD utilizes a complex carbide alloy system that provides outstanding abrasion resistance even at high temperatures. Tubular electrode design provides 90% deposition efficiency
Reduces smoke by half compared to conventional hardfacing electrodes
Runs at lower amperage reduces distortion, weld dilution andmetal fatigue
Hardness of up to 66 Rc, one layer can outlast two layers of competitive product
Designed to withstand extreme temperature abrasion up to 1400˚F (760˚C)
Not designed for impact resistance
Hardness: 63-66 Rc (deposits will relief check crack readily) Max deposit thickness: 2 layersCurrent: DCEP (DC+) or AC Abrasion resistance: Excellent ASTM G65 Procedure A (Dry sand rubber wheel abrasion test):- 10.51 mm3 volume loss- 0.072 gm mass loss For comparison sintered tungsten carbide: 0.039 to 0.080 gm mass loss
Technical Specifications
| Item#: | EG17800375 |
|---|---|
| Welding Process | Stick |
| Type | Electrode |
| Diameter | 3/8 " |
| Length | 18 " |
| Base Metal | Steel To Steel |
| Hardness | 63-66 HRC |
| Polarity | DCEP |
| UNSPSC #: | 23271810 |
| TAA Compliant: | Yes |
| Weight: | 6.17 lb |